THIS PUBLICATION HAS BEEN ARCHIVED.
Whilst this publication can still be purchased some of the information in it has been superseded by more recent research and standards. The BRE Group does not accept any responsibility whatsoever for any loss or damage, including - without limitation - indirect or consequential loss or damage arising from use, or loss of use, of data or profits arising out of, or in connection with, the use of this document.
Failure: cracking, detachment; rain penetration into structure
Defects: inadequate bond or key to wall; rendering stronger than background or preceding coats, too weak to exclude rain adequately, or too rich (or wet) to avoid cracking